MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECASINT 4111 natural Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Unfilled

Material Notes:
  • very high thermal and oxidative resistance
  • very low water absorption
  • high thermal and mechanical capacity
  • low outgassing
  • good chemical resistance
  • high creep resistance
  • resistance against high energy radiation
  • sensitive to hydrolysis in higher thermal range
Target Industries:
  • electronics
  • electrical engineering
  • conveyor technology
  • mechanical engineering
  • precision engineering
  • semiconductor technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³
Water Absorption  0.080 %
@Temperature 23.0 °C,
Time 86400 sec
0.080 %
@Temperature 73.4 °F,
Time 24.0 hour
DIN EN ISO 62
 0.30 %
@Temperature 80.0 °C,
Time 86400 sec
0.30 %
@Temperature 176 °F,
Time 24.0 hour
DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090DIN EN ISO 868
Ball Indentation Hardness 345 MPa50000 psi
Tensile Strength 100 MPa14500 psi50 mm/min; DIN EN ISO 527-1
Elongation at Break 1.7 %1.7 %10 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 6.10 GPa885 ksi1 mm/min; DIN EN ISO 527-1
Flexural Strength 160 MPa23200 psi10 mm/min; DIN EN ISO 178
Flexural Modulus 6.10 GPa885 ksi2 mm/min; DIN EN ISO 178
Compressive Strain at Break 25 %25 %10 mm/min; EN ISO 604
Compressive Yield Strength 210 MPa
@Strain 10 %
30500 psi
@Strain 10 %
10 mm/min; EN ISO 604
Compressive Strength 250 MPa36300 psi10 mm/min; EN ISO 604
Compressive Modulus 6.193 GPa898.2 ksi1 mm/min; EN ISO 604
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²max 7.5 J; DIN EN ISO 179-1
Charpy Impact, Notched 0.110 J/cm²0.523 ft-lb/in²max 7.5 J; DIN EN ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D 257
Surface Resistance 1.00e+16 ohm1.00e+16 ohmASTM D 257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 22.7 kV/mm577 kV/inASTM D149
Dissipation Factor 0.0013
@Frequency 1e+6 Hz
0.0013
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  36.0 µm/m-°C
@Temperature 50.0 - 200 °C
20.0 µin/in-°F
@Temperature 122 - 392 °F
XY; DIN 53 752
 47.0 µm/m-°C
@Temperature 200 - 300 °C
26.1 µin/in-°F
@Temperature 392 - 572 °F
XY; DIN 53 752
 52.0 µm/m-°C
@Temperature 50.0 - 200 °C
28.9 µin/in-°F
@Temperature 122 - 392 °F
Z; DIN 53 752
 65.0 µm/m-°C
@Temperature 300 - 400 °C
36.1 µin/in-°F
@Temperature 572 - 752 °F
XY; DIN 53 752
 69.0 µm/m-°C
@Temperature 200 - 300 °C
38.3 µin/in-°F
@Temperature 392 - 572 °F
Z; DIN 53 752
 99.0 µm/m-°C
@Temperature 300 - 400 °C
55.0 µin/in-°F
@Temperature 572 - 752 °F
Z; DIN 53 752
Specific Heat Capacity 1.24 J/g-°C0.296 BTU/lb-°FASTM E1461
Thermal Conductivity 0.520 W/m-K3.61 BTU-in/hr-ft²-°FASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) 470 °C878 °FASTM D 648
Flammability, UL94 V-0V-0DIN IEC 60695-11-10
Oxygen Index 53 %53 %EN ISO 4589-2
 
Descriptive Properties
Coloryellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8201 / 319129

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.