MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Mineral Filled

Material Notes: Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low warp and resistance to sink-mark formation. It maintains its inherent chemical resistance to greases, oils and hydrocarbons.

Capron 8260 HS BK-102 is generally recommended for applications such as marine hardware, brackets, fittings, bobbins, office furniture, appliance components, and power tool housings. ASTM Callout PA220 M40 A9130 KB080 AA002.

Data provided by Allied Signal.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO data
Water Absorption 1.1 %1.1 %24 hrs; ISO data
Moisture Absorption at Equilibrium 1.6 %1.6 %50% RH; 23°C; ISO data
Water Absorption at Saturation 5.7 %5.7 %in water; 23°C; ISO data
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inISO data
 0.0090 cm/cm0.0090 in/inASTM data MD
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inISO Data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 86.0 MPa12500 psiISO value at 50 mm/min.
 90.0 MPa13100 psiASTM value at 50 mm/min.
Elongation at Break 10 %10 %Nominal
 10 %10 %Nominal
Elongation at Yield 3.0 %3.0 %ASTM Value at 50 mm/min.
 3.2 %3.2 %ISO Value at 50 mm/min.
Tensile Modulus 6.63 GPa962 ksisame value from ASTM and ISO test.
Flexural Modulus 5.00 GPa725 ksiISO data
Poissons Ratio 0.350.35ISO data
Shear Modulus 2.50 GPa363 ksicalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmISO data
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature 20.0 °C
27.8 µin/in-°F
@Temperature 68.0 °F
ASTM data
Melting Point 220 °C428 °FASTM and ISO test
Deflection Temperature at 0.46 MPa (66 psi) 197 °C387 °FISO data
Deflection Temperature at 1.8 MPa (264 psi) 108 °C226 °FISO Data
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 275 °C527 °FSee Materials Notes
Mold Temperature 95.0 °C203 °FSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALC83 / 23877

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.