MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene; Linear Low Density (LLDPE)

Material Notes: Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.

Applications: Bynel® Series 4100 resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE, and ethylene copolymers. In addition, Bynel® 4107, 4109, 41E532, 41E556, 41E557, and 41E558 will also adhere to ionomers. Series 4100 resins can be used in coextrusion processes including: blown film cast film/sheet blow molding melt and solid phase thermoforming sheet and tubing Bynel® 4105, 4109, and 41E557 can also be used in coextrusion coating. LLDPE resins are known for their temperature resistance, clarity and toughness. These physical properties make the Series 4100 resins work well in applications such as: boil-in-bag structures blow molded containers in which drop strength is important bag-in-box films film where LLDPE is the heat seal layer Bynel® 4104, 4105, 4125, and 4164 provide good adhesion to EVOH and outstanding adhesion to polyamide. The primary difference between Bynel® 4104, 4105, and 4125 is their rheology. Bynel® 41E556 provides improved adhesion to EVOH and outstanding adhesion to polyamide. Bynel® 4107, 4109, 41E532, 41E557, and 41E558 provide outstanding adhesion to EVOH and polyamide. Bynel® 4107 has a low melt index, which makes it useful in blow molding and blown film processes. It provides less parison sag in blow molding and better bubble stability in blown film Bynel® 41E558 can also be used to adhere to polypropylene. In particular, Bynel® 41E532 and 41E558 provide outstanding adhesion to ionomers, particularly sodium ionomers in blown film. A potential application in a barrier/ionomer structure is oil pouches or sachets. They are also useful in cook-in applications.

Physical properties of Bynel® Series 4100 resins are typical of linear low-density polyethylene resins with similar density and melt index values. Use of these adhesive resins in coextruded PE/barrier structures offers improved thermal resistance over that of ethylene vinyl acetate-based adhesive resins. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.915 g/cc0.0331 lb/in³ASTM D792
Viscosity 1.50e+6 cP
@Shear Rate 50 1/s,
Temperature 190 °C
1.50e+6 cP
@Shear Rate 50 1/s,
Temperature 374 °F
estimated from log-log graph
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 112 °C234 °FFreezing point via DSC/ASTM D3418
 126 °C259 °FMelting point via DSC/ASTM D3418
Vicat Softening Point 100 °C212 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 235 °C455 °FExtruder forward zone and adapter for film or coating with EVA or EVOH
Nozzle Temperature 235 °C455 °FDie

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDUPBX / 33578

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.