MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese ZENITE 7755 LCP, 55% Mineral / Glass Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

Material Notes: Zenite 7755 is a 55% glass/mineral-reinforced liquid crystal polymer resin for injection molding. It has good impact resistance, excellent temperature resistance, and is suitable for applications in diverse industries.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.89 g/cc0.0683 lb/in³ISO 1183
Moisture Absorption 1.10 %1.10 %23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow 0.00 cm/cm0.00 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0010 cm/cm0.0010 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.0 %1.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 17.6 GPa2550 ksi50mm/min; ISO 527-2/1A
Flexural Strength 185 MPa26800 psiISO 178
Flexural Modulus 14.0 GPa2030 ksiISO 178
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 9.00 µm/m-°C5.00 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 39.0 µm/m-°C21.7 µin/in-°FISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 310 °C590 °FISO 75-1, -2
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
Feed Temperature 40.0 - 60.0 °C104 - 140 °F
Zone 1 355 - 365 °C671 - 689 °F
Zone 2 360 - 370 °C680 - 698 °F
Zone 3 360 - 370 °C680 - 698 °F
Zone 4 360 - 370 °C680 - 698 °F
Die Temperature 360 - 370 °C680 - 698 °F
Melt Temperature 365 - 375 °C689 - 707 °F
Drying Temperature >= 150 °C>= 302 °F
Dry Time 3.00 hour3.00 hour
Moisture Content <= 0.010 %<= 0.010 %
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Hold Pressure 50.0 - 150 MPa7250 - 21800 psi
Back Pressure <= 3.00 MPa<= 435 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zenite® 6635 BK010 LCP
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese ZENITE 6635 LCP, 40% Mineral / Glass Reinforced (Extended Stress-Strain Tabular Data)
Celanese ZENITE 6330 LCP, 30% Mineral Reinforced
Celanese ZENITE 6244L LCP, 40% Mineral / Glass Reinforced

PHCQ545 / 179000

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.