MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chambroad Petrochemicals PPS-CF40 40% Carbon Fiber Reinforced, Polyphenylene sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler

Material Notes: Modified PPS Materials: Polyphenylene sulfide (PPS) resin has a simple molecular structure and is a heat-resistant crystal polymer of the unit consisting of an aromatic ring alternated with sulfur atoms. With a melting point of about 280°C, the resin has a high resistance to heat and reagents, and can extinguish automatically without adding flame retardants. Since PPS can replace metal or thermosetting resin, it is widely applied in the fields of car parts, electrical/electronic parts, housing facilities, OA, and precision equipment.

Application Field: Aerospace - Gun shells, helmets, corrosion-resistant and wear-resistant parts of warships and submarines, aircraft connectors, coil frames, and instrument panels.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 230 MPa33400 psiISO 527-1, 2
Elongation at Break 1.0 %1.0 %ISO 527-1, 2
Tensile Modulus 32.0 GPa4640 ksiISO 527-1, 2
Flexural Strength 335 MPa48600 psiISO 178
Flexural Modulus 33.0 GPa4790 ksiISO 178
Flexural Strain at Break 1.3 %1.3 %ISO 178
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1e+05<= 1e+05IEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 265 °C509 °FISO 75-1, 2
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 305 - 330 °C581 - 626 °FBarrel
Mold Temperature 135 - 175 °C275 - 347 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAMB010 / 318552

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.