MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Toyobo Fortron® DEV FX40T1 PPS, Impact Modified
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes: Product Description: Forton DEV FX40T1 is an unreinforced, impact-modified high toughness poly(phenylene sulfide)

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Material Status: Experimental - Active

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.0 MPa6960 psiISO 527-2/50
 59.0 MPa
@Temperature -40.0 °C
8560 psi
@Temperature -40.0 °F
ISO 527-2/50
Tensile Strength, Yield 80.0 MPa
@Temperature -40.0 °C
11600 psi
@Temperature -40.0 °F
ISO 527-2/50
Tensile Modulus 2.43 GPa352 ksiISO 527-1
 2.86 GPa
@Temperature -40.0 °C
415 ksi
@Temperature -40.0 °F
ISO 527-1
Flexural Strength 84.8 MPa12300 psi3.5% strain; ISO 178
Flexural Modulus 2.80 GPa406 ksiISO 178
Poissons Ratio 0.410.41ISO 527
Charpy Impact, Notched  1.01 J/cm²
@Temperature -30.0 °C
4.80 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 5.04 J/cm²
@Temperature 22.8 °C
24.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 30.0 °C68.0 - 86.0 °FHopper
Feed Temperature 75.0 - 85.0 °C167 - 185 °FInjection
Rear Barrel Temperature 300 - 310 °C572 - 590 °F
Middle Barrel Temperature 305 - 315 °C581 - 599 °F
Front Barrel Temperature 310 - 320 °C590 - 608 °F
Nozzle Temperature 315 - 320 °C599 - 608 °F
Zone 4 310 - 320 °C590 - 608 °FInjection
Melt Temperature 315 - 320 °C599 - 608 °F
Mold Temperature 135 - 150 °C275 - 302 °F
Drying Temperature 100 °C212 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Back Pressure <= 3.50 MPa<= 508 psi
Screw Speed  50 rpm
@Thickness 55.9 mm
50 rpm
@Thickness 2.20 in
 75 rpm
@Thickness 40.6 mm
75 rpm
@Thickness 1.60 in
 120 rpm
@Thickness 24.9 mm
120 rpm
@Thickness 0.980 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6282 / 310975

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.