MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler

Material Notes: Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: excellent dimensional stability (with temperatures reaching 200°-220°C), excellent resistance to thermal ageing, high rigidity, low thermal expansion, and finally, excellent resistance to chemicals, even to very aggressive agents. Larton compounds are intrinsically self-extinguishing: they maintain UL94 V0 rating also in thin-walled products without requiring any special additive. Glass fiber reinforced Lartons require accurate design to reduce differential shrinkage and to minimize deformation of parts, but to a lower extent than with other semi-crystalline resins.

Specific Notes for this Material: UL94V-0 self-extinguishing, without halogens or phosphorus; low fume optical density and toxicity; 50% glass fiber; fair flowability; good dimensional stability; high rigidity; low coefficient of linear thermal expansion; excellent characteristics even at high temperature; excellent chemical resistance.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.71 g/cc0.0618 lb/in³ISO 1183
Water Absorption 0.010 %0.010 %at 23°C; ISO 62
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inLATI
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M >= 100>= 100ASTM D785
Tensile Strength, Ultimate 150 MPa21800 psiISO 527
 94.0 MPa
@Temperature 120 °C
13600 psi
@Temperature 248 °F
ISO 527
 120 MPa
@Temperature 90.0 °C
17400 psi
@Temperature 194 °F
ISO 527
 135 MPa
@Temperature 60.0 °C
19600 psi
@Temperature 140 °F
ISO 527
Flexural Modulus 18.0 GPa2610 ksiASTM D790
 9.55 GPa
@Temperature 120 °C
1390 ksi
@Temperature 248 °F
ASTM D790
 14.1 GPa
@Temperature 90.0 °C
2050 ksi
@Temperature 194 °F
ASTM D790
 17.45 GPa
@Temperature 60.0 °C
2531 ksi
@Temperature 140 °F
ASTM D790
Izod Impact, Notched  0.700 J/cm
@Temperature -40.0 °C
1.31 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.700 J/cm
@Temperature -20.0 °C
1.31 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.700 J/cm
@Temperature 23.0 °C
1.31 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched  1.20 J/cm²
@Temperature -20.0 °C
5.71 ft-lb/in²
@Temperature -4.00 °F
DIN 53453
 1.20 J/cm²
@Temperature -40.0 °C
5.71 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.0 kV/mm
@Thickness 2.00 mm
330 kV/in
@Thickness 0.0787 in
IEC 243-1
Comparative Tracking Index 125 V125 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 µm/m-°C
@Temperature 20.0 °C
13.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 280 °C536 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 267 °C513 °FASTM D648
Vicat Softening Point 255 °C491 °F50°C/h 50N; ISO 306
Flammability, UL94 V-0
@Thickness 0.710 mm
V-0
@Thickness 0.0280 in
Oxygen Index 46 %46 %ISO 4589
Glow Wire Test  960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 695-2-1
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 310 °C536 - 590 °F
Mold Temperature 130 - 140 °C266 - 284 °F
Drying Temperature 130 - 140 °C266 - 284 °FTemperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourDrying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)YIEC 335
Heat Resistance - Ball Test (165°C)YIEC 335
Injection Speedmedium - high
Needle Burner TestY1.47 mm
 Y3.05 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLATI255 / 50253

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.