MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Silver Birch (Gray Birch) Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Mechanical properties reported according to ASTM D143 at 12 wt% moisture content.

Key Words: Betula populifolia, timber, lumber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.600 g/cc0.600 g/ccOven-dry to green volume ratio
Density 0.552 g/cc0.0199 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 4003 N899.9 lb (f)
Modulus of Elasticity 11.86 GPa1720 ksi
Modulus of Rupture 0.08481 GPa12.30 ksi
Compressive Strength 5.10 MPa740 psiperpendicular
 39.23 MPa5690 psiparallel
Shear Strength 8.34 MPa1210 psiparallel
Work to Maximum Load 0.11032 J/cm³16.001 in-lb/in³
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Shrinkage 5.2 %5.2 %Radial, from green to oven dry, US origin
 14.7 %14.7 %Volumetric, from green to oven dry, US origin
 
Descriptive Properties
CategoryHardwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Yellow Birch Wood
Paper Birch Wood
Sweet Birch Wood
Black Maple Wood
American Maple, Rock (Sugar Maple)

PTSU076 / 100520

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.