MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Old Hickory Dunn Tennessee Ball Clay  (discontinued **)
Categories: Ceramic; Clay; Ball Clay

Material Notes: Dunn clay is a selection originating from our Gleason, TN processing facility and is characterized by moderately high levels of kaolin interspersed with the presence of some carbon content. It is an economical selection of clay that can be considered particularly where high volumes of clay may be required. The selection has an established history of performance in pavement sealer applications and structural brick compositions.

Information provided by Old Hickory Clay Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.39 µm0.39 µmMedian particle diameter
 0.50 µm0.50 µm55% of particles less than
 1.0 µm1.0 µm64% of particles less than
 <= 5.0 µm<= 5.0 µm84% of particles less than
pH 5.75.7
Soluble Sulfates 192 ppm192 ppm
Specific Surface Area 19.3 m²/g19.3 m²/g
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00310 GPa0.450 ksiDry Modulus of Rupture, 50% clay/50% flint, cast bars
 
Thermal PropertiesMetricEnglishComments
Shrinkage 5.7 %5.7 %Cone 04, Linear Fired Shrinkage
 6.4 %6.4 %Linear Drying Shrinkage
 6.5 %6.5 %Cone 3, Linear Fired Shrinkage
 7.7 %7.7 %Cone 11, Linear Fired Shrinkage
 
Component Elements PropertiesMetricEnglishComments
Al2O3 26.9 %26.9 %
CaO 0.16 %0.16 %
Fe2O3 1.0 %1.0 %
K2O 0.69 %0.69 %
Loss on Ignition(%) 8.98 %8.98 %
MgO 0.71 %0.71 %
Na2O 0.050 %0.050 %
SiO2 59.1 %59.1 %
TiO2 2.34 %2.34 %
 
Descriptive Properties
Absorption (%)10.6Cone 3, Fired
 15.8Cone 04, Fired
 3.7Cone 11, Fired
CEC/MBI (meg/100 ml)10.5
Crude ColorLight Grey
Filtration (ml)24
Pyrometric Cone Equivalent (PCE)29
Water of Plasticity (%)30
Wet Sieve Residue (%)2.29Wet Sieve Residue, +200 mesh

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EOHC914 / 161993

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.