Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing. The resin is available in transparent tint, color code 000000. A tough, transparent grade of ABS, Lustran® ABS 266 resin is used in housings, toys, lawn and garden applications, and various consumer goods.Lustran® is now a product of INEOS Styrolution. Information provided by the manufacturer. |