MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrene-Butadiene Copolymer

Customer Benefits: BK15 is an SBC consisting of our developmental BK10 grade with a mold release added for easier processing. BK15 molded parts give excellent detail on fast production cycles and are easily processed by injection molding. This resin can be tinted or colored in a variety of transparent and opaque shades. Compared to BK10, BK15 offers improved mold release with the same injection molding process conditions and equivalent molded part performance and properties. Molded parts offer excellent clarity, good toughness, good stiffness, and high surface gloss.

Applications: Major applications include molded boxes and containers, toys, displays, medical devices, overcaps, and novelties.

Processing Recommendations:
Injection Molding: Minimum melt temperature between 193-232°C necessary to permit mold fill. Minimum injection pressure required to fill the cavity. Maximum back pressure of 0.3 MPa. Drying: Generally, no need to dry resin.

Specification Data: FDA Regulations 21 CFR 177.1640; suitable for contact with non-fatty foods. [parts over 0.200 inches thick, for alcoholic beverages, or for high temperature food use (hot filled over 150°F or heat sterilized over 212°F) would require additional testing]

Data provided by Chevron Phillips Chemical Company LP.

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 200 °C
15 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ASTM D2240
Tensile Strength, Yield 21.4 MPa3100 psi2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Elongation at Break 200 %200 %2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Flexural Yield Strength 31.7 MPa4600 psiTest specimens were injection molded by ASTM D1897; ASTM D790
Flexural Modulus 1.482 GPa214.9 ksiTest specimens were injection molded by ASTM D1897; ASTM D790
Izod Impact, Notched 0.747 J/cm
@Thickness 3.17 mm
1.40 ft-lb/in
@Thickness 0.125 in
ASTM D256
Impact Test 29.7 J
@Thickness 3.17 mm
21.9 ft-lb
@Thickness 0.125 in
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FASTM D648
Vicat Softening Point 80.0 °C176 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 232 °C379 - 450 °FInjection
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® BK11 Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® CK02 Styrene-Butadiene Copolymer, Blow Molding Grade
Chevron Phillips K-Resin® XK40 Styrene-Butadiene Copolymer, Sheet Grade

PCHEVK20 / 20277

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.