MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Rynite® FR335 NC010 PET-GF35FR(30+16)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass/Mineral Reinforced

Material Notes: 35% Glass/Mineral Reinforced, Flame Retardant, Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³ISO 1183
Water Absorption 0.16 %
@Time 86400 sec
0.16 %
@Time 24.0 hour
Immersion; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiISO 527-1/-2
Elongation at Break 1.9 %1.9 %ISO 527-1/-2
Tensile Modulus 12.3 GPa1780 ksiISO 527-1/-2
Poissons Ratio 0.330.33
Charpy Impact Unnotched 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 62631-3-2
Dielectric Strength 36.0 kV/mm914 kV/inIEC 60243-1
Comparative Tracking Index 300 V300 VIEC 60112
 250 - 399 V
@Thickness 3.00 mm
250 - 399 V
@Thickness 0.118 in
PLC 2; UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FISO 11359-1/-2
 13.0 µm/m-°C
@Temperature 55.0 - 160 °C
7.22 µin/in-°F
@Temperature 131 - 320 °F
ISO 11359-1/-2
 18.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
10.0 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 64.0 µm/m-°C35.6 µin/in-°FISO 11359-1/-2
 53.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
29.4 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
 85.0 µm/m-°C
@Temperature 55.0 - 160 °C
47.2 µin/in-°F
@Temperature 131 - 320 °F
ISO 11359-1/-2
Melting Point 248 °C478 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 236 °C457 °FISO 75-1/-2
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
IEC 60695-11-10
 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
IEC 60695-11-20
Glow Wire Ignition Temperature  825 °C
@Thickness 0.750 mm
1520 °F
@Thickness 0.0295 in
IEC 60695-2-13
 900 °C
@Thickness 1.50 mm
1650 °F
@Thickness 0.0591 in
IEC 60695-2-13
 900 °C
@Thickness 3.00 mm
1650 °F
@Thickness 0.118 in
IEC 60695-2-13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 280 °C518 - 536 °FRange, Injection
Mold Temperature 110 °C230 °FOptimum, Injection
 100 - 120 °C212 - 248 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %<= 0.020 %Injection
 
Descriptive Properties
AdditivesFlame retardant
Drying RecommendedyesInjection
Part Marking Code>PET-GF35FR(30+16)<ISO 11469
PolymerPET-(GF+MD)35 FR(30+17)
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPET-GF35FR(30+16)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4845 / 256294

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.