MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Tenite Propionate 380A2R30018 Natural, Trsp Cellulose Acetate Propionate  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Propionate, Molded

Material Notes: Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.

Product Description: TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of TENITE cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. TENITE cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. TENITE Cellulose Acetate Propionate 380-18 has a plasticizer level of 18%. It is resistant to high temperatures.

Applications: Ophthalmic

Technical Data Sheet

Characteristics: Formula 380 - base

Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.

Information provided by Eastman Chemical.

Key Words: CAP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 1.4 %1.4 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 5555ASTM D785
Tensile Strength, Ultimate 27.6 MPa4000 psiASTM D638
Tensile Strength, Yield 22.1 MPa3210 psiASTM D638
Elongation at Break 35 %35 %ASTM D638
Flexural Yield Strength 29.0 MPa4210 psiASTM D790
Flexural Modulus 1.172 GPa170.0 ksiASTM D790
Izod Impact, Notched 5.23 J/cm9.80 ft-lb/inASTM D256
 1.07 J/cm
@Temperature -40.0 °C
2.00 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm1.00e+13 - 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.55
@Frequency 1e+6 Hz
3.55
@Frequency 1e+6 Hz
ASTM D 150
Dielectric Strength 15.25 kV/mm387.4 kV/inASTM D149
Dissipation Factor 0.080
@Frequency 1e+6 Hz
0.080
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 - 17.0 µm/m-°C
@Temperature 20.0 °C
6.11 - 9.44 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.465 J/g-°C0.3501 BTU/lb-°FDSC
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C171 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FConditioned 4 hours @ 70°C (158°F); ASTM D648
Vicat Softening Point 87.0 °C189 °FConditioned 4 hours @ 70°C (158°F); ASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4751.475ASTM D542
Haze <= 8.5 %
@Thickness 1.52 mm
<= 8.5 %
@Thickness 0.0598 in
ASTM D1003
Transmission, Visible >= 90 %
@Thickness 1.52 mm
>= 90 %
@Thickness 0.0598 in
ASTM E308

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate

PEA305 / 35274

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.