MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, a viscosity of 300 cps., and a weight of 7.8 lbs/gallon. AboCast 7802-1/AboCure 50-3 has versatility, many variable-ratio possibilities, and a tenacious adhesion to metals, ceramics, glass, wood, and most rigid materials which permits permanent structural and dielectric bonds. Absence of volatiles and minimum shrinkage, typical of solventless epoxy systems, allow castings and masses of virtually any desired thickness. Suggested Uses: Multi-purpose casting, coating, and bonding for applications requiring high dielectric resistance, structural strength, and radiation resistance as well as resistance to weather, water, alkalis, diluted acids, fuels, and most common solvents; it was originally developed for FERMILAB.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³AboCure 50-3
 1.09 g/cc0.0394 lb/in³AboCast 7802-1
Water Absorption 0.10 - 0.30 %0.10 - 0.30 %
Viscosity 500 - 700 cP500 - 700 cPblended
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  <= 10
@Time 86400 sec
<= 10
@Time 24.0 hour
1/8 in thickness
 20
@Time 259000 sec
20
@Time 72.0 hour
1/8 in thickness
 20
@Time 86400 sec
20
@Time 24.0 hour
 65
@Time 259000 sec
65
@Time 72.0 hour
 75
@Treatment Temp. 100 °C,
Time 10800 sec
75
@Treatment Temp. 212 °F,
Time 3.00 hour
 75
@Treatment Temp. 100 °C,
Time 10800 sec
75
@Treatment Temp. 212 °F,
Time 3.00 hour
1/8 in thickness
Tensile Strength at Break 34.5 - 48.3 MPa5000 - 7000 psi
Elongation at Break 10 - 15 %10 - 15 %
Flexural Strength 62.1 - 82.7 MPa9000 - 12000 psi
Compressive Strength 48.3 - 55.2 MPa7000 - 8000 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 15.7 - 19.7 kV/mm400 - 500 kV/in
 
Processing PropertiesMetricEnglishComments
Pot Life 300 min300 min100 g
 
Descriptive Properties
Parts by Weight (pbw)100AboCast 7802-1
 40AboCure 50-13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Cast, Unreinforced
Abatron AboCast 22-30/AboCure 50-4 Epoxy
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg
Atom Adhesives AA-BOND F110 Epoxy Adhesive
Overview of materials for Epoxy Adhesive

PABC825 / 107809

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.