MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Shakespeare Sanstat® CN125 .36mm Nylon 66 Monofilament
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66 Fiber

Material Notes: Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.

Information provided by Shakespeare Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Fiber Count 1360 dtex1220 denierPer Filament
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 32 %32 %
Tenacity 0.353 N/tex4.00 g/denier5 kg breaking load
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 9000 ohm-cm9000 ohm-cmAverage
 <= 14000 ohm-cm<= 14000 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 254 °C489 °F
Shrinkage 5.0 %
@Temperature 175 °C,
Time 601 sec
5.0 %
@Temperature 347 °F,
Time 0.167 hour
 
Descriptive Properties
Product yield7370 m/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shakespeare Sanstat® CN125 .21mm Nylon 66 Monofilament
Teknor Apex Telcar® TELC-1000-92 Thermoplastic Elastomer
Overview of materials for Nylon 66 Fiber
Morgan Advanced Ceramics Kaolite® 1600 Thermal Ceramic, Cast installation
Geon® Performance Solutions 210 Series 217 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer)

PSHAKE010 / 67289

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.