System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Durethan® TP 202-027 901510 Nylon 66 (PA66), 30% Glass/Carbon Fiber Reinforced, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Glass/Carbon Fiber Filled
Material Notes:
PA 66, 30% glass fibers/carbon fibers, injection molding, improved flowability, heat-aging stabilized, improved electrical conductivity
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.306
g/cc
0.04718
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.0028
cm/cm
0.0028
in/in
60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0077
cm/cm
0.0077
in/in
60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
Mechanical Properties
Metric
English
Comments
Puncture Resistance
700
N
@Temperature -30.0 °C
157
lb (f)
@Temperature -22.0 °F
ISO 6603-2
840
N
@Temperature 23.0 °C
189
lb (f)
@Temperature 73.4 °F
ISO 6603-2
Tensile Strength at Break
170
MPa
24700
psi
5 mm/min; ISO 527-1,-2
Elongation at Break
2.6 %
2.6 %
5 mm/min; ISO 527-1,-2
Tensile Modulus
11.8
GPa
1710
ksi
1 mm/min; ISO 527-1,-2
Flexural Strength
255
MPa
37000
psi
2 mm/min; ISO 178-A
Flexural Modulus
11.4
GPa
1650
ksi
2 mm/min; ISO 178-A
Flexural Strain at Break
2.9 %
2.9 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
10.0
kJ/m²
@Temperature 23.0 °C
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)
55.0
kJ/m²
@Temperature 23.0 °C
26.2
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
55.0
kJ/m²
@Temperature -30.0 °C
26.2
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
Charpy Impact Unnotched
5.50
J/cm²
@Temperature -30.0 °C
26.2
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
6.50
J/cm²
@Temperature 23.0 °C
30.9
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched
<=
1.00
J/cm²
@Temperature 23.0 °C
<=
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
<=
1.00
J/cm²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
Puncture Energy
2.30
J
@Temperature -30.0 °C
1.70
ft-lb
@Temperature -22.0 °F
ISO 6603-2
3.10
J
@Temperature 23.0 °C
2.29
ft-lb
@Temperature 73.4 °F
ISO 6603-2
Electrical Properties
Metric
English
Comments
Volume Resistivity
1000
ohm-cm
1000
ohm-cm
IEC 60093
Surface Resistance
10000
ohm
10000
ohm
IEC 60093
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
10.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
5.56
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow
100
µm/m-°C
@Temperature 23.0 - 55.0 °C
55.6
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point
261
°C
502
°F
10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi)
>=
250
°C
>=
482
°F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
240
°C
464
°F
ISO 75-1,-2
Shrinkage, MD
0.020 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.020 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD
0.020 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.020 %
@Treatment Temp. 248 °F,
Time 4.00 hour
60x60x2; ISO 294-4
Processing Properties
Metric
English
Comments
Melt Temperature
290
°C
554
°F
injection molding
280
-
300
°C
536
-
572
°F
Mold Temperature
80.0
°C
176
°F
injection molding
80.0
-
120
°C
176
-
248
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
2.00
-
6.00
hour
2.00
-
6.00
hour
Moisture Content
0.030 - 0.070 %
0.030 - 0.070 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled
Envalior Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber
Celanese SO.F.TER Nylfor A® A2 GFCF/30 Nylon 66
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber
Lehmann & Voss LUVOCOM® 1-0889-2 Polyamide 66 with carbon fiber and glass fiber, heat stabilized
PLANW9496 / 208376
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.