MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ATI Allvac® 38-644 UNS R58640 Titanium Alloy
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: High-strength, metastable beta alloy. Uses: Spring wire, fasteners, torsion bars for aerospace and automotive applications.

Property values are for samples in the metallurgical condition: 1600°F anneal + water quench + age.

Information provided by Allvac, An Allegheny Teledyne Company.

Key Words: AMS 4957, 4958. MIL-T-9046, 9047. MIL-F-83142.
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.81 g/cc0.174 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 3232
Tensile Strength, Ultimate 1173 MPa170100 psi
Tensile Strength, Yield 1104 MPa
@Strain 0.2 %
160100 psi
@Strain 0.2 %
Elongation at Break 8.0 %8.0 %
Reduction of Area 15 %15 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.30 %<= 0.30 %
Nitrogen, N <= 0.030 %<= 0.030 %
Oxygen, O <= 0.25 %<= 0.25 %
Palladium, Pd 0.12 - 0.25 %0.12 - 0.25 %
Titanium, Ti 99 %99 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Beta C (Ti-3Al-8V-6Cr-4Mo-4Zr) Solution Treated 815°C
Titanium Beta C (Ti-3Al-8V-6Cr-4Mo-4Zr ST 815°C, Aged 565°C
Titanium Beta C (Ti-3Al-8V-6Cr-4Mo-4Zr ST 815°C, Aged 510°C
Titanium Beta III (Ti-11.5Mo-6Zr-4.5Sn; Grade 10), Solution Treated, Unaged
Titanium Ti-11.5Mo-6Zr-4.5Sn, ST 720°C, Aged 495°C

NALLV21 / 14937

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.