MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; ECTFE Fluoropolymer

Material Notes:

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.68 g/cc1.68 g/ccASTM D792
Water Absorption at Saturation <= 0.10 %<= 0.10 %ASTM D570
Linear Mold Shrinkage, Flow 0.025 cm/cm0.025 in/inASTM D955
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090R-Scale; ASTM D785
Hardness, Shore D 7575ASTM D2240
Tensile Strength at Break 54.0 MPa
@Temperature 23.0 °C
7830 psi
@Temperature 73.4 °F
50 mm/min; ASTM D638
Tensile Strength, Yield 30.0 MPa
@Temperature 23.0 °C
4350 psi
@Temperature 73.4 °F
50 mm/min; ASTM D638
Elongation at Break 250 %
@Temperature 23.0 °C
250 %
@Temperature 73.4 °F
50 mm/min; ASTM D638
Elongation at Yield 5.0 %
@Temperature 23.0 °C
5.0 %
@Temperature 73.4 °F
50 mm/min; ASTM D638
Tensile Modulus 1.66 GPa
@Temperature 23.0 °C
241 ksi
@Temperature 73.4 °F
50 mm/min; ASTM D638
Flexural Strength 47.0 MPa
@Temperature 23.0 °C
6820 psi
@Temperature 73.4 °F
2.5 mm/min; ASTM D790
Flexural Modulus 1.69 GPa
@Temperature 23.0 °C
245 ksi
@Temperature 73.4 °F
2.5 mm/min; ASTM D790
Izod Impact, Notched  2.10 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
3.93 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
 NB
@Thickness 3.20 mm,
Temperature 23.0 °C
NB
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Coefficient of Friction, Dynamic 0.200.20vs. Itself; ASTM D1894
Coefficient of Friction, Static 0.200.20vs. Itself; ASTM D1894
Taber Abrasion, mg/1000 Cycles 5.0
@Load 0.500 kg
5.0
@Load 1.10 lb
CS-17 Wheel
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.50e+16 ohm-cm
@Temperature 23.0 °C
5.50e+16 ohm-cm
@Temperature 73.4 °F
50% RH; ASTM D257
Dielectric Constant 2.57
@Frequency 1e+6 Hz,
Temperature 23.0 °C
2.57
@Frequency 1e+6 Hz,
Temperature 73.4 °F
ASTM D150
Dielectric Strength 14.0 kV/mm
@Thickness 3.20 mm,
Temperature 23.0 °C
356 kV/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D149
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 40.0 J/g17.2 BTU/lbCrystallization Heat; ASTM D3418
 42.0 J/g18.1 BTU/lbASTM D3418
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FASTM D696
Specific Heat Capacity 0.962 J/g-°C
@Temperature 23.0 °C
0.230 BTU/lb-°F
@Temperature 73.4 °F
ASTM D3418
Thermal Conductivity 0.150 W/m-K
@Temperature 40.0 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 104 °F
ASTM C177
Melting Point 242 °C468 °FASTM D3418
Crystallization Temperature 222 °C432 °FPeak, DSC; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FUnannealed; ASTM D648
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746A
Glass Transition Temp, Tg 85.0 °C185 °FDMA
Decomposition Temperature 405 °C761 °F1% mass loss, N2; TGA
Flammability, UL94 V-0V-0UL 94
Oxygen Index 52 %52 %ASTM D2863
 
Descriptive Properties
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
FeaturesMedium Viscosity
FormsPellets
 Powder
GenericECTFE
Processing MethodExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Halar® 500 ECTFE Fluoropolymer
Syensqo (Solvay Specialty Polymers) Halar® 3404DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled
Syensqo (Solvay Specialty Polymers) Halar® 300 ECTFE Fluoropolymer
Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)
Westlake Plastics Halar® 901 ECTFE

PSOL8Y7645 / 135708

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.