LORD CoolTherm™ SC-6712/6730 silicone system is a two-component, solvent-free RTV silicone system ideal for potting and encapsulating densely packed components and for producing flexible molds. Features: maintains low viscosity for ease of component encapsulation compared to other highly thermally conductive materials. exhibits low shrinkage and stress on components as it cures. room temperature curing formulation is not subject to hardener poisoning. cured system provides excellent electrical and thermal conductivity. can be used on parts and devices that experience operating temperatures from -55°C to +205°C. All information provided by Lord. |