MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sumitomo Bakelite Sumikon® PM-9610 Phenolic, Compression Grade
Categories: Polymer; Thermoset; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: Durez “SUMIKON” PM-9610 black Phenolic is a two stage glass and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and higher dimensional stability with excellent heat resistance. Typical applications include brush holders for high temperature, and timing pulleys.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.02 g/cc2.02 g/ccASTM D792
Apparent Bulk Density 0.960 g/cc0.0347 lb/in³ASTM D1895
Water Absorption 0.030 %0.030 %ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D6289
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa13100 psiASTM D638
Tensile Modulus 25.5 GPa3700 ksiASTM D638
Flexural Strength 131 MPa19000 psiASTM D790
Compressive Strength 241 MPa35000 psiASTM D695
Izod Impact, Notched 0.214 J/cm0.401 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM D257
Dielectric Constant 4.9
@Frequency 1e+6 Hz
4.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 9.80 kV/mm249 kV/inStep by Step; ASTM D149
 14.9 kV/mm378 kV/inShort Time; ASTM D149
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C399 °FASTM D648
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Sumikon® PM-6630 Type Black Phenolic Novolac
Sumitomo Bakelite Sumikon® PM-6830 Type Black Phenolic Resol
Sumitomo Bakelite Sumikon® PM-9501 Type J Black Phenolic Novolac

PSUMIT488 / 194293

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.