MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 595°C (1100°F)
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 600 Series Stainless Steel

Material Notes: Test specimens were cold drawn and aged for 16 hours at temperature given, wire diameter of 5.61 mm, reduced in area by 22% of original diameter.

Key Words: UNS S66286 (UNS K66286), AMS 5525, AMS 5731, AMS 5732, AMS 5734, AMS 5735, AMS 5736, AMS 5737, AMS 5804, AMS 5805, ASME SA638, ASTM A453, ASTM A638, SAE J467 (A286); DIN 1.4980
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.92 g/cc0.286 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1158 MPa168000 psi
Tensile Strength, Yield 1062 MPa
@Strain 0.2 %
154000 psi
@Strain 0.2 %
Elongation at Break 21.5 %21.5 %gage length is 4 times diameter
Reduction of Area 52.5 %52.5 %
Modulus of Elasticity 200 GPa29000 ksiTypical for stainless steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.9 µm/m-°C
@Temperature 21.0 - 100 °C
9.39 µin/in-°F
@Temperature 69.8 - 212 °F
solution treated, 16.7 solution treated and aged.
 17.2 µm/m-°C
@Temperature 20.0 - 250 °C
9.56 µin/in-°F
@Temperature 68.0 - 482 °F
 17.4 µm/m-°C
@Temperature 21.0 - 500 °C
9.67 µin/in-°F
@Temperature 69.8 - 932 °F
 17.6 µm/m-°C
@Temperature 21.0 - 650 °C
9.78 µin/in-°F
@Temperature 69.8 - 1200 °F
solution treated
 17.7 µm/m-°C
@Temperature 21.0 - 750 °C
9.83 µin/in-°F
@Temperature 69.8 - 1380 °F
solution treated
 18.5 µm/m-°C
@Temperature 21.0 - 750 °C
10.3 µin/in-°F
@Temperature 69.8 - 1380 °F
solution treated and aged.
 19.4 µm/m-°C
@Temperature 21.0 - 900 °C
10.8 µin/in-°F
@Temperature 69.8 - 1650 °F
solution treated
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  12.6 W/m-K
@Temperature 21.0 °C
87.4 BTU-in/hr-ft²-°F
@Temperature 69.8 °F
 15.1 W/m-K
@Temperature 150 °C
105 BTU-in/hr-ft²-°F
@Temperature 302 °F
 20.2 W/m-K
@Temperature 425 °C
140 BTU-in/hr-ft²-°F
@Temperature 797 °F
 23.79 W/m-K
@Temperature 600 °C
165.1 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 24.7 W/m-K
@Temperature 650 °C
171 BTU-in/hr-ft²-°F
@Temperature 1200 °F
Melting Point 1370 - 1425 °C2500 - 2597 °F
Solidus 1370 °C2500 °F
Liquidus 1425 °C2597 °F
Maximum Service Temperature, Air 815 °C1500 °FContinuous Service
 980 °C1800 °FIntermittent
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.035 %<= 0.035 %
Boron, B 0.0010 - 0.010 %0.0010 - 0.010 %
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 13.5 - 16 %13.5 - 16 %
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe 56 %56 %
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 24 - 27 %24 - 27 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %
Titanium, Ti 1.9 - 2.35 %1.9 - 2.35 %
Vanadium, V 0.10 - 0.50 %0.10 - 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 425°C (800°F)
660 Stainless Steel (A286) short time tensile test
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 760°C (1400°F)
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 540°C (1000°F)
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 705°C (1300°F)

MQ660AQ / 13260

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.