MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik Vestodur® GK 20 20% Glass Bead Reinforced PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Bead Filled

Material Notes: Description: VESTODUR GK20 is a 20% glass beads-filled, semicrystalline thermoplastic polyester compound based on polybutylene terephthalate (PBT).The compound is suitable for injection molding mechanically and thermally highly stressed parts with good surface quality. Compared to unfilled PBT compounds VESTODUR GK20 shows a higher stiffness, a reduced, almost isotropic mold shrinkage, and thus a lower tendency to warp.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Water Absorption at Saturation 0.45 %0.45 %ISO 62
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
@Thickness 4.00 mm
0.012 - 0.014 in/in
@Thickness 0.157 in
sheets with film gate at rim, mold temperature 60°C
Linear Mold Shrinkage, Transverse 0.012 - 0.014 cm/cm0.012 - 0.014 in/in
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 166 MPa24100 psiH30; ISO 2039-1
Tensile Strength, Yield 60.0 MPa8700 psiISO 527-1/2
Elongation at Break 5.5 %5.5 %ISO 527-1/2
Elongation at Yield 4.0 %4.0 %ISO 527-1/2
Tensile Modulus 3.20 GPa464 ksiISO 527-1/-2
Charpy Impact Unnotched  2.20 J/cm²
@Temperature -30.0 °C
10.5 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant 3.7
@Frequency 100 Hz
3.7
@Frequency 100 Hz
IEC 60250
Dielectric Strength 27.0 kV/mm686 kV/inK20/P50; IEC 60243-1
Dissipation Factor 0.010
@Frequency 100 Hz
0.010
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 225 V225 V100 drops value; IEC 60112
 250 V250 VTest Solution A CTI; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C
@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Temperature 73.4 - 131 °F
Longitudinal; ISO 11359, DIN 53752
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359, DIN 53752
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C162 °FISO 75-1/-2
Vicat Softening Point 193 °C379 °FMethod B, 50 N; ISO 306
 215 °C419 °FMethod A, 10 N; ISO 306
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695
 
Descriptive Properties
Electrolytic CorrosionA1IEC 60426

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUMA32 / 47546

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.