MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

EMS-Grivory Grilamid® LV-15H nat Nylon 12, 15% Glass Fiber Filled, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Filler/Reinforcement: Glass Fiber, 15% Filler by Weight

Additive: Impact Modifier; UV Stabilizer

Features: High Impact Resistance; Hydrolysis Resistant; Impact Modified; UV Stabilized

Uses: Appliance; Automotive Applications; Automotive Electronics; Automotive Lighting; Connectors; Consumer Applications; Electrical/Electronic Applications; Engineering Parts; Hydraulic Applications; Industrial Applications; Medical Devices; Pneumatic Applications

RoSH Compliance: RoSH Compliant

Automotive Specifications: ASTM D4066 PA420 G15 A99940 KB055 UA024 PA080 Color: 9733 Black

Appearance: Natural Color

Forms: Granules

Processing Method: Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Water Absorption 0.80 %0.80 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 1.3 %1.3 %ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0030 cm/cm0.0030 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 74
@Time 15.0 sec
74
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 70.3 MPa10200 psiISO 527-2
Elongation at Break 10 %10 %ISO 527-2
Tensile Modulus 3.00 GPa435 ksiISO 527-1
Charpy Impact Unnotched  7.56 J/cm²
@Temperature -30.0 °C
36.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 7.56 J/cm²
@Temperature 22.8 °C
36.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.01 J/cm²
@Temperature -30.0 °C
4.80 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.49 J/cm²
@Temperature 22.8 °C
7.10 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Strength 35.0 kV/mm890 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60012

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM155 / 307514

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.