MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Resinoid 2010 Phenolic Molding, Fabric Reinforced  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Fabric Filled

Material Notes: Data provided by the manufacturer.

The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ASTM D792A
Water Absorption 1.1 %1.1 %24 hours R.T. ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inPositive Mold; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8686ASTM D785
Hardness, Rockwell M 112112ASTM D785
Tensile Strength, Ultimate 41.0 MPa5950 psiASTM D651
Flexural Strength 69.0 MPa10000 psiASTM D790
Flexural Modulus 11.0 GPa1600 ksiASTM D790
Compressive Strength 145 MPa21000 psiASTM D695
Izod Impact, Notched 0.683 J/cm1.28 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 10.0 kV/mm254 kV/inShort Time; Dry; ASTM D149
Comparative Tracking Index 175 - 250 V
@Thickness 3.05 mm
175 - 250 V
@Thickness 0.120 in
UL PLC 4 (100-175 V)
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness 3.05 mm
60 - 120 sec
@Thickness 0.120 in
UL PLC 1; UL PLC 1
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 3.05 mm
>= 120 arcs
@Thickness 0.120 in
UL PLC 0; UL PLC 0
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
@Thickness 3.05 mm
>= 5.91 in/min
@Thickness 0.120 in
UL PLC 4 (150+ mm/min)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °FUL RTI
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FASTM D648
UL RTI, Electrical 150 °C302 °F
UL RTI, Mechanical with Impact 150 °C302 °F
UL RTI, Mechanical without Impact 150 °C302 °F
 
Processing PropertiesMetricEnglishComments
Mold Temperature 155 - 180 °C311 - 356 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Novolac, Fabric Filled
Vyncolit W5020 Glass Filled Novolac Phenolic
Resinoid 2002-4 Phenolic Molding, Fabric Reinforced
Hippe PF CC 21 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube

PPHR0J / 56242

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.