MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Mobility and Materials Delrin® 100CPE BK602 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: High Viscosity Acetal Homopolymer with Very Low Emissions

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Melt Density 1.18 g/cc
@Temperature 205 °C
0.0426 lb/in³
@Temperature 401 °F
Linear Mold Shrinkage, Flow 0.021 cm/cm0.021 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inISO 294-4, 2577
Melt Flow  2.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
cm³/10min Volumetric; ISO 1133
 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 72.0 MPa10400 psiISO 527-1/-2
Elongation at Break 40 %40 %Nominal; ISO 527-1/-2
Elongation at Yield 21 %21 %ISO 527-1/-2
Tensile Modulus 3.10 GPa450 ksiISO 527-1/-2
Poissons Ratio 0.370.37
Charpy Impact Unnotched  30.0 J/cm²
@Temperature -30.0 °C
143 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 35.0 J/cm²
@Temperature 23.0 °C
167 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 °C392 °FOptimum, Extrusion
 195 - 205 °C383 - 401 °FRange, Extrusion
 200 - 210 °C392 - 410 °FRange, Injection
 205 °C401 °FOptimum, Injection
Mold Temperature 90.0 °C194 °FOptimum, Injection
 80.0 - 100 °C176 - 212 °FInjection
Drying Temperature 80.0 °C176 °FInjection
 75.0 - 85.0 °C167 - 185 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Extrusion
 <= 0.20 %<= 0.20 %Injection
Hold Pressure 90.0 - 110 MPa13100 - 16000 psiInjection
 110 MPa16000 psiInjection
Annealing Temperature 160 °C320 °FOptional; 30 min + 5 min/mm of thickness
 
Descriptive Properties
Annealing time (min/mm)30optional; 30 min + 5 min/mm of thickness
Drying RecommendedyesInjection
Emissions (mg/kg)<2VDA 275
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>POM<ISO 11469
PolymerPOM
Processing Hold Pressure Time (s/mm)8Injection
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPOMISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5083ea / 290905

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.