MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Sheet/Thermoforming Grade

Material Notes: Extra High Molecular Weight Hexene Copolymer

Formolene® HL5010 has good melt strength, excellent stress crack resistance, good rigidity, and excellent impact strength even at low temperatures. These properties make Formolene® HL5010 an excellent resin for large part blow molding applications.

Formolene® HL5010 meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520 for food packaging, covering safe use of polyolefin articles intended for direct food contact.

Applications: Blow Molded - 55-Gallon Shipping Containers, Gasoline Tanks and Agricultural Chemical Tanks; Extruded – Pallets, Cattle Feeders, Large Formed Parts and Boats

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.949 g/cc0.0343 lb/in³ASTM D1505
ESCR 100% Igepal® >= 600 hour>= 600 hourCondition A, F50; ASTM D1693
ESCR 10% Igepal® >= 600 hour>= 600 hourCondition B, F50; ASTM D1693
High Load Melt Index 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
10 g/10 min
@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.8 MPa3600 psi2" (50mm) per min, Type IV; ASTM D638
Elongation at Break >= 600 %>= 600 %2" (50mm) per min, Type IV; ASTM D638
Flexural Modulus 1.17 GPa170 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -91.0 °C<= -132 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM 5502-01 Polyethylene, Sheet/Thermoforming Grade, HDPE
Chevron Phillips Marlex® HHM 5202 Polyethylene, Sheet/Thermoforming Grade, HDPE
LyondellBasell Petrothene® LR732001 High Density Polyethylene, Sheet & Profile Data
LyondellBasell Petrothene® LP500210 High Density Polyethylene (Sheet & Profile Grade)
Formosa Plastics Formolene® HL3721 Sheet and Thermoforming HDPE

PFPCPQ061 / 150293

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.