MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 3104-H19
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A93104; Aluminium 3104-H19; AA3104-H19; Al3104-H19
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.72 g/cc0.0983 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7878500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 101101Converted from Brinell Hardness Value
Hardness, Vickers 8888Converted from Brinell Hardness Value
Tensile Strength, Ultimate 290 MPa42100 psi
Tensile Strength, Yield 260 MPa37700 psi
Elongation at Break 4.0 %
@Thickness 1.60 mm
4.0 %
@Thickness 0.0630 in
In 5 cm
Modulus of Elasticity 69.0 GPa10000 ksiAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus. Estimated from trends in similar Al alloys.
Poissons Ratio 0.340.34Estimated from trends in similar Al alloys.
Shear Modulus 26.0 GPa3770 ksiEstimated from similar Al alloys.
Shear Strength 175 MPa25400 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000400 ohm-cm0.00000400 ohm-cmEstimated from trends in similar Al alloys.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.8 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
 25.4 µm/m-°C
@Temperature 20.0 - 300 °C
14.1 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°FEstimated from trends in similar Al alloys.
Thermal Conductivity 170 W/m-K1180 BTU-in/hr-ft²-°FEstimated from trends in similar Al alloys.
Melting Point 630 - 655 °C1170 - 1210 °FEstimated from trends in similar Al alloys.
Solidus 630 °C1170 °FEstimated from trends in similar Al alloys.
Liquidus 655 °C1210 °FEstimated from trends in similar Al alloys.
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 95 - 98.4 %95 - 98.4 %As remainder
Copper, Cu 0.05 - 0.25 %0.05 - 0.25 %
Gallium, Ga <= 0.05 %<= 0.05 %
Iron, Fe <= 0.80 %<= 0.80 %
Magnesium, Mg 0.80 - 1.3 %0.80 - 1.3 %
Manganese, Mn 0.80 - 1.4 %0.80 - 1.4 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.60 %<= 0.60 %
Titanium, Ti <= 0.10 %<= 0.10 %
Vanadium, V <= 0.05 %<= 0.05 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 3004-H19
6111 Aluminum Composition Spec
Aluminum 5182-H32
Aluminum 3003-H112
Aluminum 3105-O

MA3104H19 / 9035

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.