MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Vestolit® Pulver 5421 PVC-HI  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, High Impact

Material Notes: For window sections to be printed or laminated with foil.

ISO data as provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³
Water Absorption 3.0 %3.0 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 5.0 %5.0 %
Modulus of Elasticity 2.50 GPa363 ksi
Tensile Impact Strength 170 kJ/m²80.9 ft-lb/in²
Tensile Creep Modulus, 1 hour 2400 MPa348000 psi
Tensile Creep Modulus, 1000 hours 1000 MPa145000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
Vicat Softening Point 81.0 °C178 °F50°C/hr/50 N

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene CP0435G20HIV Copolymer Glass Reinforced High Impact
Aclo Accucomp Polystyrene HS0600L High Impact
Aclo Accucomp ABS ABS856BL High Flow Medium Impact Grade
Aclo Accucomp ABS ABS846HL High Flow Medium Impact Grade
Aclo Accucomp ABS ABS812L High Impact Grade

PHUM47 / 47480

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.