MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Gharda Chemicals G-PAEK™ 1230FC Ultra High Performance PEK Polymer
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Carbon Fiber Filled

Material Notes: Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in color

Application Areas: Suitable for high temperature application, where higher strength & stiffness needed in load bearing application. Excellent wear resistance. Chemically resistant to aggressive environments, suitable for sterilization for medical and food contact applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/cc
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
Linear Mold Shrinkage, Flow 0.0011 cm/cm0.0011 in/in410°C nozzle, 220°C mold
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in410°C nozzle, 220°C mold
Crystallinity 40 %40 %DSC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 106106ASTM D785
Hardness, Shore D 9191
Tensile Strength at Break  45.0 MPa
@Temperature 250 °C
6530 psi
@Temperature 482 °F
ASTM D638
 55.0 MPa
@Temperature 200 °C
7980 psi
@Temperature 392 °F
ASTM D638
 80.0 MPa
@Temperature 150 °C
11600 psi
@Temperature 302 °F
ASTM D638
 120 MPa
@Temperature 100 °C
17400 psi
@Temperature 212 °F
ASTM D638
 130 - 135 MPa
@Temperature 23.0 °C
18900 - 19600 psi
@Temperature 73.4 °F
ASTM D638
 145 MPa
@Temperature -10.0 °C
21000 psi
@Temperature 14.0 °F
ASTM D638
 160 MPa
@Temperature -50.0 °C
23200 psi
@Temperature -58.0 °F
ASTM D638
Elongation at Break 1.5 - 2.0 %1.5 - 2.0 %ASTM D638
Tensile Modulus 11.5 GPa1670 ksiASTM D638
Flexural Strength 210 MPa30500 psiASTM D790
Flexural Modulus 10.5 GPa1520 ksiASTM D790
Izod Impact, Notched 0.400 - 0.450 J/cm0.749 - 0.843 ft-lb/inASTM D256
Izod Impact, Unnotched 6.10 J/cm11.4 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 370 - 372 °C698 - 702 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 368 °C694 °F
Glass Transition Temp, Tg 152 - 154 °C306 - 309 °FDSC/onset
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 390 - 425 °C734 - 797 °F
Nozzle Temperature 425 °C797 °F
Mold Temperature 200 - 220 °C392 - 428 °F
Drying Temperature 150 °C302 °F
Dry Time 4 - 6 hour4 - 6 hour
 
Descriptive Properties
Hopper/ Throat Temperature60-80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gharda Chemicals G-PAEK™ 1230CF Ultra High Performance PEK Polymer
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Evonik VESTAKEEP® 4000CF30 PEEK
Shell Carilon® DP P1000 Polyketone
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled

PGHARD994 / 108529

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.