Description: Polyoxymethylene based batch with approx. 20% silicone (polysiloxane) for modifying tribological properties of thermoplastic polyoxymethylenes. Recommended concentrations of batch FK66003 within the mixture with thermoplastic polyoxymethylenes are in the range of 1 to 5.Information provided by BASF |