MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Perstorp Compounds AMITEC VXO UF/MF blend
Categories: Polymer; Thermoset; Melamine

Material Notes: A special Urea Formaldehyde/Melamine Formaldehyde blend that enhances surface properties and is optimized for cost-effective injection molding of visible components.

Information provided by Perstorp Compounds Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ISO 1183
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/inDIN 53 464
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 2.4 %2.4 %ISO 178
Flexural Strength >= 130 MPa>= 18900 psiISO 178
Charpy Impact Unnotched >= 1.40 J/cm²>= 6.66 ft-lb/in²ISO 179
Charpy Impact, Notched >= 0.140 J/cm²>= 0.666 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmDIN 53 483
Surface Resistance >= 1.00e+10 ohm>= 1.00e+10 ohmDIN 53 482
Dielectric Constant 5.05.0DIN 53 483
Dissipation Factor <= 0.10
@Frequency 1000 Hz
<= 0.10
@Frequency 1000 Hz
DIN 53 483
Comparative Tracking Index >= 600 V>= 600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 160 °C>= 320 °FISO 175
Deflection Temperature at 8.0 MPa >= 100 °C>= 212 °FISO 175
Flammability, UL94 V-0V-0
Shrinkage 0.80 - 1.1 %0.80 - 1.1 %Post Shrinkage; DIN 53 464
 
Descriptive Properties
Glow Bar 960°C 180 secBH2-8IEC 707
Water Absorption [mg]<200DIN 53 495/23°C 96h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler
Overview of materials for Vinyl Ester Sheet Molding Compound
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
Overview of materials for Thermoset Polyurethane Foam, Glass Filled

PPERST10 / 56187

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.