MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Carbon Fiber Filled

Material Notes: Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in color

Application Areas: Suitable for high temperature application, where higher strength & stiffness needed in load bearing application. Excellent wear resistance. Typical applications include electronic chip carrier trays, conductive flooring, and parts for electronic business machines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/cc
Water Absorption 0.070 %
@Time 86400 sec
0.070 %
@Time 24.0 hour
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/in410°C nozzle, 220°C mold
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/in410°C nozzle, 220°C mold
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 104104ASTM D785
Hardness, Shore D 8787
Tensile Strength, Yield 160 MPa23200 psiASTM D638
Elongation at Break 2.3 %2.3 %ASTM D638
Tensile Modulus 16.0 GPa2320 ksiASTM D638
Flexural Strength 250 MPa36300 psiASTM D790
Flexural Modulus 12.9 GPa1870 ksiASTM D790
Izod Impact, Notched 0.350 - 0.400 J/cm0.656 - 0.749 ft-lb/inASTM D256
Izod Impact, Unnotched 3.50 J/cm6.56 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+8 ohm-cm1.00e+8 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+6 ohm1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 370 - 372 °C698 - 702 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 340 °C644 °F
Glass Transition Temp, Tg 152 - 154 °C306 - 309 °FDSC/onset
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 390 - 425 °C734 - 797 °F
Nozzle Temperature 425 °C797 °F
Mold Temperature 200 - 220 °C392 - 428 °F
Drying Temperature 150 °C302 °F
Dry Time 4 - 6 hour4 - 6 hour
 
Descriptive Properties
Hopper/ Throat Temperature60-80°C
Nominal Granule Diameter2.0 - 3.5 mmGranules of uniform cut and color
Nominal Granule Length2.0 - 4.0 mmNo longs greater than 8.0 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ WG101 Polyaryletherketone
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)
LATI Latamid 12 CP/85 PA 12
LATI Latigray 82-02 CX/80 PA 12
Overview of materials for PEKK, Unreinforced

PGHARD990 / 108525

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.