MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS); Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³
 1.24 g/cc0.0448 lb/in³
Filler Content 25 %25 %
 25 %25 %
Moisture Absorption 0.010 %0.010 %24 hrs., 50% RH
 0.010 %0.010 %24 hrs., 50% RH
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in
 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in
 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psi
 125 MPa18100 psi
Elongation at Break 2.3 %2.3 %
 2.3 %2.3 %
Tensile Modulus 8.20 GPa1190 ksi
 8.20 GPa1190 ksi
Flexural Yield Strength 195 MPa28300 psi
 195 MPa28300 psi
Flexural Modulus 7.80 GPa1130 ksi
 7.80 GPa1130 ksi
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²
 13.0 kJ/m²6.19 ft-lb/in²
Izod Impact, Unnotched (ISO) 43.0 kJ/m²20.5 ft-lb/in²
Charpy Impact Unnotched 4.70 J/cm²22.4 ft-lb/in²
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 24.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
13.3 µin/in-°F
@Temperature -22.0 - 86.0 °F
CTE, linear, Transverse to Flow 39.0 µm/m-°C21.7 µin/in-°F
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °F
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °F
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 310 °C536 - 590 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F
 
Descriptive Properties
CommentsNSF61
 SPS blend optimized for ductility & fatigue resistance

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled

PIDEM100 / 171616

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.