MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Universal Wire Works Au-Pd-Ni (AMS 4786) Gold Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Solder/Braze Alloy

Material Notes: Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 1005 - 1037 °C1841 - 1899 °F
Solidus 1005 °C1841 °F
Liquidus 1037 °C1899 °F
 
Component Elements PropertiesMetricEnglishComments
Gold, Au 70 %70 %
Nickel, Ni 22 %22 %
Palladium, Pd 8.0 %8.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Universal Wire Works Au-Pd-Ni (AMS 4784) Gold Brazing Filler Metal
Morgan Advanced Ceramics Mac-35 Au/65 Cu-WM Braze Alloy
Universal Wire Works BAu-5 (AMS 4785) Gold Brazing Filler Metal
Silver-Copper Eutectic Alloy (72Ag-28Cu; UNS P07720; AWS BAg-8), Cold Drawn then Annealed at 250°C (480°F)
Indium Corp. Indalloy 211 Ag-Cu Solder Alloy

NUWW250 / 19711

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.