MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LG Chemical TR580 MABS, Injection Molding Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: Transparency, Chemical Resistance

Applications: Chemical Resistance

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 2.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
2.5 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 39.0 MPa
@Thickness 3.20 mm
5660 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 15 %
@Thickness 3.20 mm
15 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Tensile Modulus 1.60 GPa
@Thickness 3.20 mm
232 ksi
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Strength 64.0 MPa
@Thickness 3.20 mm
9280 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 1.80 GPa
@Thickness 3.20 mm
262 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  0.200 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
0.375 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 0.200 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
0.375 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 0.800 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.50 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 0.800 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
1.50 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
@Thickness 6.40 mm
174 °F
@Thickness 0.252 in
Unannealed, Edgewise; ASTM D648
Vicat Softening Point 87.0 °C
@Load 5.00 kg
189 °F
@Load 11.0 lb
50°C/h; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 1.2 %1.2 %ASTM D1003
Transmission, Visible 90 %
@Thickness 3.20 mm
90 %
@Thickness 0.126 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 230 °C410 - 446 °F
Middle Barrel Temperature 220 - 240 °C428 - 464 °F
Front Barrel Temperature 230 - 250 °C446 - 482 °F
Nozzle Temperature 230 - 260 °C446 - 500 °F
Melt Temperature 220 - 250 °C428 - 482 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 90.0 °C
@Time 7200 - 14400 sec
176 - 194 °F
@Time 2.00 - 4.00 hour
Moisture Content >= 0.010 %>= 0.010 %
Back Pressure 2.94 - 5.88 MPa426 - 853 psi
Screw Speed 30 - 80 rpm30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical TR558A MABS, Injection Molding Grade
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness
LG Chemical TR557 MABS, High Transparency, High Impact
LG Chemical TR556 MABS, Transparency, Chemical Resistance
LG Chemical TR552 MABS, Transparency, High Impact, Chemical Resistance

PLHCHEM9959 / 239475

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.