MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Röchling LAMINEX® 2100 Cotton Fabric, Phenolic Resin Impregnated
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Fabric Filled

Material Notes: Application: bearing shells and bearing collars

Information provided by Schwartz Technical Plastics GmbH. Schwartz was acquired by Röchling in 2018.

Key Words: PF-7708
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO R 1183
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 130 MPa18900 psiHc 30; ISO 2039; partially
Tensile Strength, Yield 60.0 MPa8700 psiISO-DIS 527
Tensile Modulus 6.00 - 8.00 GPa870 - 1160 ksiDIN 53457
Flexural Strength 80.0 MPa11600 psiDIN 54352
Compressive Strength 150 MPa21800 psiISO 604
Izod Impact, Notched (ISO) 18.0 kJ/m²8.57 ft-lb/in²DIN 53453
Izod Impact Resistance 2.50 J/cm²11.9 ft-lb/in²swinging hammer 0,1 DIN 51222; DIN 53453
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.05.0DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 - 30.0 µm/m-°C
@Temperature 20.0 - 100 °C
8.33 - 16.7 µin/in-°F
@Temperature 68.0 - 212 °F
DIN 53752
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 125 °C257 °FContinuous
 150 °C302 °FIntermittent
 
Descriptive Properties
Creepage/leakage ResistanceKC100DIN 53480
Moisture Absorption at Equilibrium450 mgDIN 53472

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta MC330 Phenolic Cotton Laminate Sheet
Human Compact Bone, Haversian System
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Femur
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets

PSCHW037 / 90234

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.