MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties
Categories: Metal; Ferrous Metal; Tool Steel; Oil-Hardening Steel

Material Notes: Data provided by Carpenter Technology Corporation.

This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture toughness. This alloy has been used in gears where temperature resistance is important.

Pyrowear® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS K71040
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Estimated by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 334334Estimated from Rockwell C for 3000 kg load, 10 mm ball Brinell measurement.
Hardness, Knoop 363363Estimated from Rockwell C
Hardness, Rockwell C 3636
Hardness, Vickers 349349Estimated from Rockwell C
Tensile Strength, Ultimate 1172 MPa170000 psi
 1207 MPa
@Temperature 177 °C
175100 psi
@Temperature 351 °F
 1331 MPa
@Temperature -54.0 °C
193000 psi
@Temperature -65.2 °F
Tensile Strength, Yield 965 MPa140000 psiOffset not given
 896 MPa
@Temperature 177 °C
130000 psi
@Temperature 351 °F
Offset not given
 1103 MPa
@Temperature -54.0 °C
160000 psi
@Temperature -65.2 °F
Offset not given
Elongation at Break 16 %16 %
 12 %
@Temperature 177 °C
12 %
@Temperature 351 °F
 18 %
@Temperature -54.0 °C
18 %
@Temperature -65.2 °F
Reduction of Area 66.5 %66.5 %
 46 %
@Temperature 177 °C
46 %
@Temperature 351 °F
 63 %
@Temperature -54.0 °C
63 %
@Temperature -65.2 °F
Fracture Toughness 130 MPa-m½118 ksi-in½K(Q)
Charpy Impact 130 J95.9 ft-lbV-notch
 55.0 J
@Temperature -54.0 °C
40.6 ft-lb
@Temperature -65.2 °F
V-notch
 155 J
@Temperature 177 °C
114 ft-lb
@Temperature 351 °F
V-notch
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.26 µm/m-°C
@Temperature 24.0 - 93.0 °C
6.256 µin/in-°F
@Temperature 75.2 - 199 °F
 12.06 µm/m-°C
@Temperature 24.0 - 260 °C
6.700 µin/in-°F
@Temperature 75.2 - 500 °F
 13.05 µm/m-°C
@Temperature 24.0 - 538 °C
7.250 µin/in-°F
@Temperature 75.2 - 1000 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.10 %0.10 %
Chromium, Cr 1.0 %1.0 %
Copper, Cu 2.0 %2.0 %
Iron, Fe 89.5 %89.5 %as remainder
Manganese, Mn 0.35 %0.35 %
Molybdenum, Mo 3.25 %3.25 %
Nickel, Ni 2.0 %2.0 %
Silicon, Si 1.0 %1.0 %
Vanadium, V 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe Lescalloy® 9310 VAC-ARC Premium Carburizing Steel
ATI Allvac® Vasco® 9310 Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization
ATI Allvac® 9310 UNS G93106, UNS H93100 Specialty Steel
Aluminum 6082-T6
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core

NCARK0 / 15798

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.