MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.

Unibar 400-15 is not recommended for Hardening and Tempering.

Information provided by United Cast Bar Ltd.

Key Words: EN-1563-GJS-400-15 GGG40; Meehanite SF400
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.30 g/cc0.264 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 140 - 190
@Load 3000 kg
140 - 190
@Load 6610 lb
10 mm ball
Tensile Strength  370 MPa
@Diameter 105 - 200 mm
53700 psi
@Diameter 4.13 - 7.87 in
 370 MPa
@Diameter 205 - 600 mm
53700 psi
@Diameter 8.07 - 23.6 in
 390 MPa
@Diameter 55.0 - 100 mm
56600 psi
@Diameter 2.17 - 3.94 in
 400 MPa
@Diameter 25.0 - 50.0 mm
58000 psi
@Diameter 0.984 - 1.97 in
Tensile Strength, Yield  240 MPa
@Diameter 105 - 200 mm,
Strain 0.2 %
34800 psi
@Diameter 4.13 - 7.87 in,
Strain 0.2 %
 240 MPa
@Diameter 205 - 600 mm,
Strain 0.2 %
34800 psi
@Diameter 8.07 - 23.6 in,
Strain 0.2 %
 250 MPa
@Diameter 25.0 - 50.0 mm,
Strain 0.2 %
36300 psi
@Diameter 0.984 - 1.97 in,
Strain 0.2 %
 250 MPa
@Diameter 55.0 - 100 mm,
Strain 0.2 %
36300 psi
@Diameter 2.17 - 3.94 in,
Strain 0.2 %
Elongation at Break  11 %
@Thickness 105 - 200 mm
11 %
@Thickness 4.13 - 7.87 in
 11 %
@Thickness 205 - 600 mm
11 %
@Thickness 8.07 - 23.6 in
 14 %
@Thickness 55.0 - 100 mm
14 %
@Thickness 2.17 - 3.94 in
 15 %
@Thickness 25.0 - 50.0 mm
15 %
@Thickness 0.984 - 1.97 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.25 - 3.7 %3.25 - 3.7 %
Iron, Fe 92.83 - 94.19 %92.83 - 94.19 %as balance
Magnesium, Mg 0.040 - 0.070 %0.040 - 0.070 %
Manganese, Mn 0.10 - 0.30 %0.10 - 0.30 %
Phosphorus, P 0.015 - 0.080 %0.015 - 0.080 %
Silicon, Si 2.4 - 3.0 %2.4 - 3.0 %
Sulfur, S 0.0050 - 0.020 %0.0050 - 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 600-3 Continuously Cast Spheroidal Graphite Iron
Overview of materials for Gray Cast Iron
United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron

NUNITED06 / 160453

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.