MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Tubes
Categories: Polymer; Thermoset; Melamine

Material Notes: Description: Mechanical and electrical applications. Arc-resistant and tracking-resistant material. Good flame resistance. Self-extinguishing. Halogen-free. Lower high-voltage values and insulation resistance than the other G-Etronax types.

Information provided by Elektro-Isola

Key Words: IEC/EN 61212-3-1 MF GC 21, DIN 7735 Hgw 2275, NEMA LI G-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc
@Thickness >=0.000 mm
0.0650 lb/in³
@Thickness >=0.000 in
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3
Water Absorption 0.10 %0.10 %24hr/50°C+24hr in water at 23°C; ISO 62-1; IEC/EN 61212-2 7.2
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 300 MPa
@Diameter >=100 mm
43500 psi
@Diameter >=3.94 in
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1
Compressive Strength 180 MPa
@Temperature 23.0 °C,
Time 86400 sec
26100 psi
@Temperature 73.4 °F,
Time 24.0 hour
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Adhesive Bond Strength 250 MPa
@Diameter <=100 mm
36300 psi
@Diameter <=3.94 in
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+8 ohm
@Diameter 8.00 - 10.0 mm
1.00e+8 ohm
@Diameter 0.315 - 0.394 in
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2
Dielectric Constant  6.0
@Frequency 50 Hz
6.0
@Frequency 50 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
 6.0
@Frequency 1e+6 Hz
6.0
@Frequency 1e+6 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
Dielectric Strength 3.30 kV/mm
@Thickness 3.00 mm
83.8 kV/in
@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
 1.20 kV/mm
@Diameter >=3.00 mm
30.5 kV/in
@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Dissipation Factor  0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
 0.020
@Frequency 50 Hz
0.020
@Frequency 50 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 130 °C
@Thickness 3.00 mm,
Time 7.20e+7 sec
266 °F
@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10; IEC/EN 61212-2 7.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si), Aged
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si)
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy
Solvay CORFIL® 615 Potting Compound
Pyrotek TS-105 Thermoset Electrical Insulation Product (Nema Grade: G-5)

PELEKT017 / 126893

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.