MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

EOS PA 1101 Nylon 11
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Unreinforced

Material Notes: The white, light-transmissive, additively manufactured parts are characterized by high impact resistance and elongation at break. They do not splinter even under the highest mechanical loads. Compared to PA 12, they have higher temperature resistance and nearly constant mechanical properties over a wide temperature range. The material PA 1101 is based on renewable resources (castor oil).

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 48.0 MPa6960 psi
Elongation at Break 45 %45 %
Tensile Modulus 1.60 GPa232 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 201 °C394 °F20°C/min
Deflection Temperature at 0.46 MPa (66 psi) 180 °C356 °F
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C115 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEOS902 / 280562

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.