MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Hexcel® HexPEKK® EM for SLS Printing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; PEKK, Unreinforced

Material Notes: Description: HexPEKK® EM is a low resistivity, absorptive material developed for additive manufacturing with selective laser sintering (SLS) technology. The material has several orders of magnitude improved resistivity compared to the HexPEKK® 100 formula and can be used in applications where electrostatic discharge or EM shielding are design drivers.

Information provided by Hexcel Corporation.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 62.1 MPa9010 psiZ
 75.2 MPa10900 psiXY
Elongation at Break 1.59 %1.59 %Z
 1.94 %1.94 %XY
Tensile Modulus 4.688 GPa679.9 ksiZ
 4.743 GPa687.9 ksiXY
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3820 ohm-cm3820 ohm-cm
Surface Resistivity per Square 8.43 ohm8.43 ohm
 
Thermal PropertiesMetricEnglishComments
Melting Point 300 °C572 °FASTM D3418
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -184 °C-299 °F
Glass Transition Temp, Tg 160 °C320 °FASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9598 / 322752

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.