MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECATEC PPS CF50 T200 CP/IP/OS V01 natural PPS, 50% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 50% Carbon Fiber Filler

Material Notes:
  • electrically insulating
  • inherent flame resistance
  • excellent mechanical properties
  • continuous service temperature up to 150 °C
Target Industries:
  • automotive industry
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³
Filler Content 50 %50 %Fiber volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 680 MPa98600 psiISO 527-4
Modulus of Elasticity 55.0 GPa7980 ksiISO 527-4
Flexural Strength 780 MPa113000 psiISO 14125
Flexural Modulus 57.0 GPa8270 ksiISO 14125
Compressive Strength 650 MPa94300 psiISO 14126
Compressive Modulus 51.0 GPa7400 ksiISO 14126
Shear Strength 131 MPa19000 psiInterplanar; ISO 14129
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 5.00 µm/m-°C2.78 µin/in-°F
CTE, linear, Transverse to Flow 5.00 µm/m-°C2.78 µin/in-°F
Melting Point 285 °C545 °F
Maximum Service Temperature, Air 230 °C446 °Flong term
 260 °C500 °Fshort term
Glass Transition Temp, Tg 90.0 °C194 °F
 
Processing PropertiesMetricEnglishComments
Drying Temperature 150 °C302 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
 
Descriptive Properties
Colornatural
Fiber volume content (%)50
General material information0.22 mmply thickness (consolidated)
 1000 mmMaterial widths
 1270 mmMaterial widths
 200 g/m²Fiber areal weight
 349 g/m²Areal weight finished product
 carbon HT 3kFiber type
 Twill 2/2Fiber architecture
Resin weight content (%)42.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8254 / 319182

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.