MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Goodfellow Iron 40/Nickel 38/Boron 18 Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.90 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 740740kg(f)/mm²
Tensile Strength at Break >= 700 MPa>= 102000 psi
Tensile Modulus 64.0 GPa9280 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000138 ohm-cm0.000138 ohm-cm
Magnetic Coercive Force, Hc 0.10 Oe0.10 Oe
Magnetic Saturation Flux Density, Bmax 8800 Gauss8800 Gauss
Magnetic Remanence, Br 0.68 Gauss0.68 GaussRemanence Ratio, Br/Bs
Curie Temperature 353 °C667 °F
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature 410 °C770 °F
Maximum Service Temperature, Air 125 °C257 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 18 %18 %
Iron, Fe 40 %40 %
Molybdenum, Mo 4.0 %4.0 %
Nickel, Ni 38 %38 %
 
Descriptive Properties
Saturation magnetostriction (x10^-6)12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Iron 77.5/Boron 15/Silicon 7.5 Alloy
AIM CASTIN Solder for Photonic Packaging
AIM 96.5Sn/3.5Ag Solder for Photonic Packaging
AIM 95Sn/3.5Ag/1.5In Solder for Photonic Packaging
AIM 91Sn/9Zn Solder for Photonic Packaging

NGOODF159 / 16231

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.