MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Torlon® 5030 PAI, 30% glass fiber
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Glass Filled

Material Notes: 30% glass fiber, high stiffness, high strength, good retention of stiffness at high temperatures, very low creep

Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics similar to aluminum and therefore excellent dimensional stability.

Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep and chemicals.

The mechanical properties of Torlon® 5030 resin make it a candidate for metal replacement in high temperature, high stress applications. In addition, it offers outstanding electrical properties, which makes it ideal for high performance parts such as connectors, switches and relays.

- High Flow: Torlon® 5030-HF
- Low Flow: Torlon® 5030-LF
- Extrusion Grade: Torlon® 5030-E

Applications: Aerospace Applications; Aircraft Applications; Automotive Applications; Business Equipment; Connectors; Electrical Housing; Electrical Parts; Electrical/Electronic Applications; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Oil/Gas Applications; Sealing Devices; Switches; Valves/Valve Parts

Features: Chemical Resistant; Creep Resistant; Flame Retardant; Good Compressive Strength; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Temperature Strength

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.61 g/cc0.0582 lb/in³ASTM D792
Water Absorption 0.24 %
@Time 86400 sec
0.24 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0025 cm/cm0.0010 - 0.0025 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 221 MPa32100 psiASTM D638
Tensile Stress 205 MPa29700 psiASTM D1708
Tensile Modulus 14.5 GPa2100 ksiASTM D638
Flexural Strength  181 MPa
@Temperature 232 °C
26300 psi
@Temperature 450 °F
ASTM D790
 333 MPa
@Temperature 23.0 °C
48300 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus  9.86 GPa
@Temperature 232 °C
1430 ksi
@Temperature 450 °F
ASTM D790
 11.7 GPa
@Temperature 23.0 °C
1700 ksi
@Temperature 73.4 °F
ASTM D790
Compressive Strength 264 MPa38300 psiASTM D695
Compressive Modulus 7.93 GPa1150 ksiASTM D695
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256
Izod Impact, Unnotched 5.30 J/cm9.93 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+17 ohm-cm2.00e+17 ohm-cmASTM D257
Surface Resistance 1.00e+18 ohm1.00e+18 ohmASTM D257
Dielectric Constant  4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
ASTM D150
 4.4
@Frequency 60 Hz
4.4
@Frequency 60 Hz
ASTM D150
Dielectric Strength 33.0 kV/mm838 kV/inASTM D149
Dissipation Factor  0.022
@Frequency 60 Hz
0.022
@Frequency 60 Hz
ASTM D150
 0.050
@Frequency 1e+6 Hz
0.050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C8.89 µin/in-°FASTM D696
Thermal Conductivity 0.360 W/m-K2.50 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 282 °C540 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 304 °C579 °F
Nozzle Temperature 371 °C700 °F
Mold Temperature 199 - 216 °C390 - 421 °F
Drying Temperature 177 °C
@Time 10800 sec
351 °F
@Time 3.00 hour
Moisture Content <= 0.050 %<= 0.050 %Injection
Back Pressure 6.89 MPa999 psi
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw L/D Ratio, Injection18.0:1.0 to 24.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4551 / 280351

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.