MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Trinseo CALIBRE™ SF 7070 Polycarbonate, 7% Glass Reinforced Structural Foam Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Foam

Material Notes: CALIBRE® SF7070. is a 7% glass reinforced structural foam ignition resistant polycarbonate resin specially developed for injection molding processing. The CALIBRE 7070 resin provides a high flexural modulus and dimensional stability while maintaining processability and high impact strength. CALIBRE SF7070 is UL listed.

CALIBRE SF7070 structural foam resin is typically used for components of transportation equipment, internal machine structures and business machine housings.

Available Melt Flow Rate: 15.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM Data
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/in
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
15 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psiASTM Data
Elongation at Break 6.0 %6.0 %ASTM Data
Tensile Modulus 2.28 GPa331 ksiASTM Data
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 56.7 µm/m-°C
@Temperature 20.0 °C
31.5 µin/in-°F
@Temperature 68.0 °F
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 143 °C289 °FUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 134 °C273 °FUnannealed; ASTM Data
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
UL94 V-0/5V

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
Trinseo CALIBRE™ 2061 HD 15 Polycarbonate Resin

PZZDW041 / 34272

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.