MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Westlake Plastics Pomalux® CN-SS Acetal Copolymer (conductive)  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Steel Filled

Material Notes: Stainless-steel-fiber-filled, non-sloughing, dimensionally stable material HDT @ 264 psi of 225F. This material has relatively high chemical resistance, is extremely strong and stiff, and is an excellent choice for situations where carbon-based conductive fillers are not acceptable. Easily machined with carbide-tipped tooling to tight tolerances.

Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

New suppliers have been added for this product during the past 60 days.  

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686ASTM D2240
Tensile Strength, Yield 59.3 MPa8600 psiASTM D638
Flexural Strength 89.6 MPa13000 psiASTM D790
Flexural Modulus 2.76 GPa400 ksiASTM D790
Izod Impact, Notched 0.374 J/cm0.700 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 1.00e+6 ohm-cm100 - 1.00e+6 ohm-cmDry; ASTM D257
Surface Resistance 100 - 1.00e+6 ohm100 - 1.00e+6 ohmDry; ASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 88.2 µm/m-°C
@Temperature 20.0 °C
49.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 107 °C225 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive)
Ensinger Tecamid® GF30 Extruded Nylon 6/6 30% glass-fiber-reinforced (PA66)
Ensinger ENSILON® 6/6 GF30 Extruded Nylon 6/6, 30% glass-fiber-reinforced (PA66)
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
ELM® NSF H1 Food Grade Chain and Cable Lubricant

PWEST057 / 72737

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.