MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt HANDY HI-TEMP 095 Carbide Brazing Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes:

Applications:Handy Hi-Temp 095 is a ductile copper-nickel-manganese filler metal designed for intermediate temperature brazing of carbides, cast irons, steel, stainless steels and nickel base heat-resistant alloys. This filler metal is ideally suited for combined brazing/heat-treating. It is useful in the brazing of materials that may be harmed by the higher temperatures used in copper brazing. It also may be used to advantage in the brazing of materials that are subject to erosion and grain-boundary penetration associated with high boron (2 to 5%) brazing filler metals.

Characteristics:This filler metal is relatively free-flowing and will flow into long, narrow joints, except when solution of excessive amounts of nickel raises the liquidus temperature. Preferred joint clearances are in the range of 0.001 to 0.003 in. (3 to 8mm). Fluxless brazing may be accomplished in dry hydrogen or argon of at least -80EF (-62EC) dew point or by vacuum at 10-3 torr or better.

Specifications:This filler metal conforms to the following specification-SAE AMS-4764

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.67 g/cc0.277 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  225 - 393 MPa
@Temperature 427 °C
32700 - 57000 psi
@Temperature 800 °F
304 Stainless Steel torch brazed butt joint
 325 - 404 MPa
@Temperature 427 °C
47200 - 58600 psi
@Temperature 800 °F
304 Stainless Steel furnace brazed butt joint
 354 - 412 MPa
@Temperature 23.0 °C
51300 - 59700 psi
@Temperature 73.4 °F
 421 - 462 MPa
@Temperature 427 °C
61000 - 67000 psi
@Temperature 800 °F
4140 Carbon Steel torch brazed butt joint
 371 - 590 MPa
@Temperature 23.0 °C
53800 - 85600 psi
@Temperature 73.4 °F
 403 - 589 MPa
@Temperature 23.0 °C
58400 - 85400 psi
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000129 ohm-cm0.000129 ohm-cmSoft Wire
 
Thermal PropertiesMetricEnglishComments
Melting Point 879.4 - 927 °C1615 - 1700 °F
Solidus 879.4 °C1615 °FMelting Point
Liquidus 927 °C1700 °FFlow Point
 
Processing PropertiesMetricEnglishComments
Processing Temperature 954 - 1090 °C1750 - 2000 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Boron, B <= 0.10 %<= 0.10 %
Copper, Cu 51.5 - 53.5 %51.5 - 53.5 %
Iron, Fe <= 0.10 %<= 0.10 %
Manganese, Mn >= 36.3 %>= 36.3 %
Nickel, Ni 8.5 - 10.5 %8.5 - 10.5 %
Other, total <= 0.50 %<= 0.50 %
 
Descriptive Properties
ColorReddish Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AMG Aluminum 60% Manganese Aluminum Alloy
Universal Wire Works AMS 4764 Silver Brazing Filler Metal
Aluminum 1100-O
Aluminum 1100-H19 Foil
Aluminum 1100-H18

NLUCMI10 / 18077

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.