RT500M is composed of a medium weight glass fabric combined with an epoxy resin system. RT500M combines excellent electrical characteristics with very good physical properties. Electrical properties maintained in high humidity conditions. It also complies with MIL-I-24768/2, Type GEE and ASTM D709 Type IV Grade G-10. RT500M is not flame resistant.Information provided by Norplex-Micarta |
Fiber Glass, Epoxy, Micarta, NEMA G-10, MIL-I-24768/2 Type GEE, ASTM D709 Type IV Grade G-10 |