MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Glass fiber Filled; UHMW PE (Ultra High Molecular Weight PE)

Material Notes: The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from the surface give a rounded and hard sliding surface. This material is used for applications that involve manufacturing and transportation at high pressure.

Special Properties:
• Protects the sliding partner
• Extremely good resistance to chemicals
• Approved for use in the food industry (EU and FDA

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PE-UHMW
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density <= 0.940 g/cc<= 0.0340 lb/in³ISO 1183
Moisture Absorption at Equilibrium <= 0.010 %<= 0.010 %ISO 62
Water Absorption at Saturation <= 0.010 %<= 0.010 %ISO 62
Molecular Weight 9.00e+6 g/mol9.00e+6 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565DIN 53505
Ball Indentation Hardness 44.0 MPa6380 psi
Tensile Strength at Break >= 29.0 MPa>= 4210 psiISO 527
Tensile Strength 25.0 MPa3630 psiISO 527
Elongation at Break 290 %290 %ISO 527
Modulus of Elasticity 0.700 GPa102 ksi
Compressive Yield Strength  9.50 MPa
@Strain 1 %
1380 psi
@Strain 1 %
ISO 604
 15.0 MPa
@Strain 2 %
2180 psi
@Strain 2 %
ISO 604
 24.0 MPa
@Strain 5.0 %
3480 psi
@Strain 5.0 %
ISO 604
Charpy Impact, Notched >= 10.0 J/cm²>= 47.6 ft-lb/in²ISO 179
Coefficient of Friction, Dynamic 0.10 - 0.200.10 - 0.20
Sand Slurry 8080value in %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Strength <= 45.0 kV/mm<= 1140 kV/inIEC 60243
 
Thermal PropertiesMetricEnglishComments
CTE, linear 170 µm/m-°C
@Temperature 23.0 - 60.0 °C
94.4 µin/in-°F
@Temperature 73.4 - 140 °F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FISO 52612
Melting Point 130 - 135 °C266 - 275 °FISO 3146
Maximum Service Temperature, Air 90.0 °C194 °FShort Term
 80.0 °C
@Time 1.80e+7 sec
176 °F
@Time 5000 hour
Minimum Service Temperature, Air -200 °C-328 °F
Glass Transition Temp, Tg -120 °C-184 °F
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorLight Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR® Xtended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet)
Röchling Polystone® M MPG Glass filled UHMW-PE
Beijing Evergrow Resources UHMW PE Fiber Rope
Mitsubishi Chemical Advanced Materials TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Linings (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet)

PMURT913 / 156560

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.