MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.

Unibar 500-7 can be hardened by conventional methods.

Information provided by United Cast Bar Ltd.

Key Words: EN-1563-GJS-500-7 GGG50; Meehanite SFP500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.30 g/cc0.264 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170 - 230
@Load 3000 kg
170 - 230
@Load 6610 lb
10 mm ball
Tensile Strength  420 MPa
@Diameter 105 - 200 mm
60900 psi
@Diameter 4.13 - 7.87 in
 420 MPa
@Diameter 205 - 600 mm
60900 psi
@Diameter 8.07 - 23.6 in
 450 MPa
@Diameter 55.0 - 100 mm
65300 psi
@Diameter 2.17 - 3.94 in
 500 MPa
@Diameter 25.0 - 50.0 mm
72500 psi
@Diameter 0.984 - 1.97 in
Tensile Strength, Yield  290 MPa
@Diameter 105 - 200 mm,
Strain 0.2 %
42100 psi
@Diameter 4.13 - 7.87 in,
Strain 0.2 %
 290 MPa
@Diameter 205 - 600 mm,
Strain 0.2 %
42100 psi
@Diameter 8.07 - 23.6 in,
Strain 0.2 %
 300 MPa
@Diameter 55.0 - 100 mm,
Strain 0.2 %
43500 psi
@Diameter 2.17 - 3.94 in,
Strain 0.2 %
 320 MPa
@Diameter 25.0 - 50.0 mm,
Strain 0.2 %
46400 psi
@Diameter 0.984 - 1.97 in,
Strain 0.2 %
Elongation at Break  5.0 %
@Thickness 105 - 200 mm
5.0 %
@Thickness 4.13 - 7.87 in
 5.0 %
@Thickness 205 - 600 mm
5.0 %
@Thickness 8.07 - 23.6 in
 7.0 %
@Thickness 25.0 - 50.0 mm
7.0 %
@Thickness 0.984 - 1.97 in
 7.0 %
@Thickness 55.0 - 100 mm
7.0 %
@Thickness 2.17 - 3.94 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.25 - 3.7 %3.25 - 3.7 %
Iron, Fe 92.83 - 94.19 %92.83 - 94.19 %as balance
Magnesium, Mg 0.040 - 0.070 %0.040 - 0.070 %
Manganese, Mn 0.10 - 0.30 %0.10 - 0.30 %
Phosphorus, P 0.015 - 0.080 %0.015 - 0.080 %
Silicon, Si 2.4 - 3.0 %2.4 - 3.0 %
Sulfur, S 0.0050 - 0.020 %0.0050 - 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 600-3 Continuously Cast Spheroidal Graphite Iron
Gray Cast Iron, ASTM A 48 Class 40

NUNITED07 / 160454

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.